Section 218.204 Emission
Limitations
Except as provided in Sections
218.205, 218.207, 218.208, 218.212, 218.215 and 218.216 of this Subpart, no
owner or operator of a coating line shall apply at any time any coating in
which the VOM content exceeds the following emission limitations for the specified
coating. Except as otherwise provided in subsections (a), (c), (g), (h), (j), (l),
(n), (p), and (q) of this Section, compliance with the emission limitations
marked with an asterisk in this Section is required on and after March 15,
1996, and compliance with emission limitations not marked with an asterisk is
required until March 15, 1996. The following emission limitations are expressed
in units of VOM per volume of coating (minus water and any compounds which are
specifically exempted from the definition of VOM) as applied at each coating
applicator, except where noted. Compounds which are specifically exempted from
the definition of VOM should be treated as water for the purpose of calculating
the "less water" part of the coating composition. Compliance with
this Subpart must be demonstrated through the applicable coating analysis test
methods and procedures specified in Section 218.105(a) of this Part and the
recordkeeping and reporting requirements specified in Section 218.211(c) of
this Subpart except where noted. (Note: The equation presented in Section
218.206 of this Part shall be used to calculate emission limitations for
determining compliance by add-on controls, credits for transfer efficiency,
emissions trades and cross-line averaging.) The emission limitations are as
follows:
a)
|
Automobile or Light-Duty Truck
Coating
|
kg/l
|
lb/gal
|
|
|
|
|
|
1)
|
Prior to May 1, 2012:
|
|
|
|
|
|
A)
|
Prime coat
|
0.14
|
(1.2)
|
|
|
|
0.14*
|
(1.2)*
|
|
|
|
B)
|
Primer surface coat
|
1.81
|
(15.1)
|
|
|
|
1.81*
|
(15.1)*
|
BOARD NOTE: The primer surface
coat limitation is in units of kg (lbs) of VOM per l (gal) of coating solids
deposited. Compliance with the limitation shall be based on the daily-weighted
average from an entire primer surfacer operation. Compliance shall be demonstrated
in accordance with the topcoat protocol referenced in Section 218.105(b)(1)(A)
and the recordkeeping and reporting requirements specified in Section
218.211(f). Testing to demonstrate compliance shall be performed in accordance
with the topcoat protocol and a detailed testing proposal approved by the
Agency and USEPA specifying the method of demonstrating compliance with the
protocol. Section 218.205 does not apply to the primer surfacer limitation.
|
|
C)
|
Topcoat
|
kg/l
|
lb/gal
|
|
|
|
1.81
|
(15.1)
|
|
|
|
1.81*
|
(15.1)*
|
BOARD NOTE: The topcoat
limitation is in units of kg (lbs) of VOM per l (gal) of coating solids
deposited. Compliance with the limitation shall be based on the daily-weighted
average from an entire topcoat operation. Compliance shall be demonstrated in
accordance with the topcoat protocol referenced in Section 218.105(b)(1)(A) of
this Part and the recordkeeping and reporting requirements specified in Section
218.211(f). Testing to demonstrate compliance shall be performed in accordance
with the topcoat protocol and a detailed testing proposal approved by the
Agency and USEPA specifying the method of demonstrating compliance with the
protocol. Section 218.205 of this Part does not apply to the topcoat
limitation.
|
|
D)
|
Final repair coat
|
kg/l
|
lb/gal
|
|
|
|
0.58
|
(4.8)
|
|
|
|
0.58*
|
(4.8)*
|
2) On
and after May 1, 2012, subject automobile and light-duty truck coating lines
shall comply with the following limitations. These limitations shall not apply
to materials supplied in containers with a net volume of 0.47 liters (16 oz) or
less, or a net weight of 0.45 kg (1 lb) or less:
A) Electrodeposition
primer (EDP) operations. For purposes of this subsection (a)(2)(A),
"electrodeposition" means a water-borne dip coating process in which
opposite electrical charges are applied to the substrate and the coating. The
coating is attracted to the substrate due to the electrochemical potential
difference that is created.
|
|
|
kg VOM/l coating solids
applied
|
lb VOM/gal coating solids
applied
|
|
|
|
|
|
|
|
|
i)
|
When solids turnover ratio (RT)
is greater than or equal to 0.160
|
0.084
|
(0.7)
|
|
|
|
|
|
|
|
|
ii)
|
When RT is greater
than or equal to 0.040 and less than 0.160
|
0.084 x
3500.160-RT
|
(0.084 x 3500.160-RT
x 8.34)
|
|
|
|
|
|
|
|
B)
|
Primer surfacer operations
|
kg VOM/l coating solids
deposited
|
lb VOM/gal coating solids
deposited
|
|
|
|
|
|
|
|
|
|
|
i)
|
VOM content limitation
|
1.44
|
(12.0)
|
|
|
|
|
|
|
|
|
|
|
ii)
|
Compliance with the limitation
set forth in subsection (a)(2)(B)(i) shall be based on the daily-weighted
average from an entire primer surfacer operation. Compliance shall be
demonstrated in accordance with the topcoat protocol referenced in Section
218.105(b)(1)(B) and the recordkeeping and reporting requirements specified
in Section 218.211(f). Testing to demonstrate compliance shall be performed
in accordance with the topcoat protocol and a detailed testing proposal
approved by the Agency and USEPA specifying the method of demonstrating
compliance with the protocol. Section 218.205 does not apply to the primer
surfacer limitation.
|
|
|
|
|
|
|
|
|
|
C)
|
Topcoat operations
|
kg VOM/l coating solids
deposited
|
lb VOM/gal coating solids
deposited
|
|
|
|
|
|
|
|
|
|
i)
|
VOM content limitation
|
1.44
|
(12.0)
|
|
|
|
|
|
|
|
|
|
ii)
|
Compliance with the limitation
set forth in subsection (a)(2)(C)(i) shall be based on the daily-weighted
average from an entire topcoat operation. Compliance shall be demonstrated
in accordance with the topcoat protocol referenced in Section
218.105(b)(1)(B) and the recordkeeping and reporting requirements specified
in Section 218.211(f). Testing to demonstrate compliance shall be performed
in accordance with the topcoat protocol and a detailed testing proposal
approved by the Agency and USEPA specifying the method of demonstrating
compliance with the protocol. Section 218.205 does not apply to the topcoat
limitation.
|
|
|
|
|
|
|
|
|
D)
|
Combined primer surfacer and
topcoat operations
|
kg VOM/l coating solids
deposited
|
lb VOM/gal coating solids
deposited
|
|
|
|
|
|
|
|
|
|
i)
|
VOM content limitation
|
1.44
|
(12.0)
|
|
|
|
|
|
|
|
|
|
ii)
|
Compliance with the limitation
set forth in subsection (a)(2)(D)(i) shall be based on the daily-weighted
average from the combined primer surfacer and topcoat operations. Compliance
shall be demonstrated in accordance with the topcoat protocol referenced in
Section 218.105(b)(1)(B) and the recordkeeping and reporting requirements
specified in Section 218.211(f). Testing to demonstrate compliance shall be
performed in accordance with the topcoat protocol and a detailed testing
proposal approved by the Agency and USEPA specifying the method of
demonstrating compliance with the protocol. Section 218.205 does not apply
to the combined primer surfacer and topcoat limitation.
|
|
|
|
|
|
|
|
|
E)
|
Final repair coat operations
|
kg/l coatings
|
lb/gal coatings
|
|
|
|
|
|
|
|
|
|
i)
|
VOM content limitation
|
0.58
|
(4.8)
|
|
|
|
|
|
|
|
|
|
|
ii)
|
Compliance with the final
repair operations limitation set forth in subsection (a)(2)(E)(i) shall be on
an occurrence-weighted average basis, calculated in accordance with the
equation below, in which clear coatings shall have a weighting factor of 2
and all other coatings shall have a weighting factor of 1. For purposes of
this subsection (a)(2)(E)(ii), an "occurrence" is the application
of the combination of coatings that constitute a final repair coat for a
single automobile or light-duty truck. Section 218.205 does not apply to the
final repair coat limitation.
|
|
|
|
|
|
|
|
|
where:
VOMtot
|
=
|
Total VOM content of all
coatings, as applied, on an occurrence weighted average basis, and used to
determine compliance with this subsection (a)(2)(E).
|
i
|
=
|
Subscript denoting a specific
coating applied.
|
n
|
=
|
Total number of coatings
applied in the final repair operation, other than clear coatings.
|
VOMcc
|
=
|
The VOM content, as applied,
of the clear coat used in the final repair operation.
|
VOMi
|
=
|
The VOM content of each
coating used in the final repair operation, as applied, other than clear coatings.
|
F) Miscellaneous
Materials. For reactive adhesives subject to this subsection (a)(2)(F),
compliance shall be demonstrated in accordance with the methods and procedures
set forth in appendix A to Subpart PPPP of 40 CFR 63, incorporated by reference
in Section 218.112 of this Part.
|
kg/l
|
lb/gal
|
i)
|
Glass bonding primer
|
0.90
|
(7.51)
|
|
|
|
|
ii)
|
Adhesive
|
0.25
|
(2.09)
|
|
|
|
|
iii)
|
Cavity wax
|
0.65
|
(5.42)
|
|
|
|
|
iv)
|
Trunk sealer
|
0.65
|
(5.42)
|
|
|
|
|
v)
|
Deadener
|
0.65
|
(5.42)
|
|
|
|
|
vi)
|
Gasket/gasket sealing material
|
0.20
|
(1.67)
|
|
|
|
|
vii)
|
Underbody coating
|
0.65
|
(5.42)
|
|
|
|
|
viii)
|
Trunk interior coating
|
0.65
|
(5.42)
|
|
|
|
|
ix)
|
Bedliner
|
0.20
|
(1.67)
|
|
|
|
|
x)
|
Weatherstrip adhesive
|
0.75
|
(6.26)
|
|
|
|
|
xi)
|
Lubricating wax/compound
|
0.70
|
(5.84)
|
b)
|
Can Coating
|
kg/l
|
lb/gal
|
|
|
1)
|
Sheet basecoat and overvarnish
|
|
|
|
|
|
A)
|
Sheet basecoat
|
0.34
|
(2.8)
|
|
|
|
|
0.26*
|
(2.2)*
|
|
|
|
B)
|
Overvarnish
|
0.34
|
(2.8)
|
|
|
|
|
0.34
|
(2.8)*
|
|
|
2)
|
Exterior basecoat and
overvarnish
|
0.34
|
(2.8)
|
|
|
|
0.25*
|
(2.1)*
|
|
3)
|
Interior body spray coat
|
|
|
|
|
|
A)
|
Two piece
|
0.51
|
(4.2)
|
|
|
|
|
0.44*
|
(3.7)*
|
|
|
|
B)
|
Three piece
|
0.51
|
(4.2)
|
|
|
|
|
0.51*
|
(4.2)*
|
|
|
4)
|
Exterior end coat
|
0.51
|
(4.2)
|
|
|
|
0.51*
|
(4.2)*
|
|
|
5)
|
Side seam spray coat
|
0.66
|
(5.5)
|
|
|
|
0.66*
|
(5.5)*
|
|
|
|
|
|
|
6)
|
End sealing compound coat
|
0.44
|
(3.7)
|
|
|
|
0.44*
|
(3.7)*
|
c)
|
Paper Coating
|
|
|
|
|
|
|
|
|
1)
|
Prior to May 1, 2011:
|
kg/l
|
lb/gal
|
|
|
|
0.28
|
(2.3)
|
|
|
|
|
|
|
|
|
2)
|
On and after May 1, 2011:
|
kg VOM/kg
|
kg VOM/kg
|
|
|
|
(lb VOM/lb)
|
(lb
VOM/lb)
|
|
|
|
solids
applied
|
coatings
applied
|
|
|
|
|
A)
|
Pressure sensitive tape and
label surface coatings
|
0.20
|
(0.067)
|
|
|
|
|
B)
|
All other paper coatings
|
0.40
|
(0.08)
|
|
|
|
|
|
|
|
3) The
paper coating limitation set forth in this subsection (c) shall not apply to
any owner or operator of any paper coating line on which flexographic,
rotogravure, lithographic, or letterpress printing is performed if the paper
coating line complies with the applicable emissions limitations in Subpart H of
this Part. In addition, screen printing on paper is not regulated as paper
coating, but is regulated under Subpart TT of this Part. On and after May 1,
2011, the paper coating limitation shall also not apply to coating performed on
or in-line with any digital printing press, or to size presses and on-machine
coaters on papermaking machines applying sizing or water-based clays.
d)
|
Coil Coating
|
|
kg/l
|
lb/gal
|
|
|
|
0.31
|
(2.6)
|
|
|
|
0.20*
|
(1.7)*
|
|
|
|
e)
|
Fabric Coating
|
0.35
|
(2.9)
|
|
|
|
0.28*
|
(2.3)*
|
|
|
|
f)
|
Vinyl Coating
|
0.45
|
(3.8)
|
|
|
|
0.28*
|
(2.3)*
|
|
|
|
g)
|
Metal Furniture Coating
|
|
|
|
|
|
|
1)
|
Prior to May 1, 2011:
|
|
|
|
|
|
|
kg/l
|
lb/gal
|
|
|
|
A)
|
Air dried
|
0.34
|
(2.8)
|
|
|
|
|
|
B)
|
Baked
|
0.28
|
(2.3)
|
|
|
|
|
2)
|
On and after May 1, 2011:
|
|
|
|
|
|
|
kg/l
(lb/gal)
|
kg/l (lb/gal)
solids applied
|
|
|
|
A)
|
General, One-Component
|
0.275
|
0.40
|
|
|
|
|
|
(2.3)
|
(3.3)
|
|
|
|
|
|
B)
|
General, Multi-Component
|
|
|
|
|
|
|
|
|
i)
|
Air dried
|
0.340
|
0.55
|
|
|
|
|
|
|
(2.8)
|
(4.5)
|
|
|
|
|
|
|
ii)
|
Baked
|
0.275
|
0.40
|
|
|
|
|
|
|
(2.3)
|
(3.3)
|
|
|
|
|
|
C)
|
Extreme High Gloss
|
|
|
|
|
|
|
|
|
i)
|
Air dried
|
0.340
|
0.55
|
|
|
|
|
|
|
(2.8)
|
(4.5)
|
|
|
|
|
|
|
ii)
|
Baked
|
0.360
|
0.61
|
|
|
|
|
|
|
(3.0)
|
(5.1)
|
|
|
|
|
|
D)
|
Extreme Performance
|
|
|
|
|
|
|
|
|
i)
|
Air dried
|
0.420
|
0.80
|
|
|
|
|
|
|
(3.5)
|
(6.7)
|
|
|
|
|
|
|
ii)
|
Baked
|
0.360
|
0.61
|
|
|
|
|
|
|
(3.0)
|
(5.1)
|
|
|
|
|
|
E)
|
Heat Resistant
|
|
|
|
|
|
|
|
i)
|
Air dried
|
0.420
|
0.80
|
|
|
|
|
|
(3.5)
|
(6.7)
|
|
|
|
|
ii)
|
Baked
|
0.360
|
0.61
|
|
|
|
|
|
(3.0)
|
(5.1)
|
|
|
|
F)
|
Metallic
|
0.420
|
0.80
|
|
|
|
|
|
|
(3.5)
|
(6.7)
|
|
|
|
G)
|
Pretreatment Coatings
|
0.420
|
0.80
|
|
|
|
|
|
|
(3.5)
|
(6.7)
|
|
|
|
H)
|
Solar Absorbent
|
|
|
|
|
|
|
|
i)
|
Air dried
|
0.420
|
0.80
|
|
|
|
|
|
(3.5)
|
(6.7)
|
|
|
|
|
ii)
|
Baked
|
0.360
|
0.61
|
|
|
|
|
|
(3.0)
|
(5.1)
|
|
|
|
|
|
|
|
|
|
|
3) On
and after May 1, 2011, the limitations set forth in this subsection (g) shall
not apply to stencil coatings, safety-indicating coatings, solid-film
lubricants, electric-insulating and thermal-conducting coatings, touch-up and
repair coatings, or coating applications utilizing hand-held aerosol cans.
h)
|
Large Appliance Coating
|
|
1)
|
Prior to May 1, 2011:
|
kg/l
|
lb/gal
|
|
A)
|
Air dried
|
0.34
|
(2.8)
|
|
B)
|
Baked
|
0.28
|
(2.3)
|
|
2)
|
On and after May 1, 2011:
|
kg/l
|
kg/l (lb/gal)
|
|
|
|
(lb/gal)
|
solids applied
|
|
A)
|
General, One Component
|
0.275
|
0.40
|
|
|
|
(2.3)
|
(3.3)
|
|
B)
|
General, Multi-Component
|
|
|
|
|
i)
|
Air dried
|
0.340
|
0.55
|
|
|
|
(2.8)
|
(4.5)
|
|
|
ii)
|
Baked
|
0.275
|
0.40
|
|
|
|
(2.3)
|
(3.3)
|
|
C)
|
Extreme High Gloss
|
|
|
|
|
i)
|
Air dried
|
0.340
|
0.55
|
|
|
|
(2.8)
|
(4.5)
|
|
|
ii)
|
Baked
|
0.360
|
0.61
|
|
|
|
(3.0)
|
(5.1)
|
|
D)
|
Extreme Performance
|
|
|
|
|
i)
|
Air dried
|
0.420
|
0.80
|
|
|
|
(3.5)
|
(6.7)
|
|
|
ii)
|
Baked
|
0.360
|
0.61
|
|
|
|
(3.0)
|
(5.1)
|
|
E)
|
Heat Resistant
|
|
|
|
|
i)
|
Air dried
|
0.420
|
0.80
|
|
|
|
(3.5)
|
(6.7)
|
|
|
ii)
|
Baked
|
0.360
|
0.61
|
|
|
|
|
(3.0)
|
(5.1)
|
|
F)
|
Metallic
|
0.420
|
0.80
|
|
|
|
(3.5)
|
(6.7)
|
|
G)
|
Pretreatment Coatings
|
0.420
|
0.80
|
|
|
|
(3.5)
|
(6.7)
|
|
H)
|
Solar Absorbent
|
|
|
|
|
i)
|
Air dried
|
0.420
|
0.80
|
|
|
|
(3.5)
|
(6.7)
|
|
|
ii)
|
Baked
|
0.360
|
0.61
|
|
|
|
|
(3.0)
|
(5.1)
|
|
|
|
|
|
|
|
|
|
3) The
limitations set forth in this subsection (h) shall not apply to the use of
quick-drying lacquers for repair of scratches and nicks that occur during
assembly, provided that the volume of coating does not exceed 0.95 1 (1 quart)
in any one rolling eight-hour period. On and after May 1, 2011, these
limitations shall also not apply to stencil coatings, safety-indicating
coatings, solid-film lubricants, electric-insulating and thermal-conducting
coatings, touch-up and repair coatings, or coating applications utilizing
hand-held aerosol cans.
i)
|
Magnet Wire Coating
|
|
kg/1
|
lb/gal
|
|
|
0.20
|
(1.7)
|
|
|
0.20*
|
(1.7)*
|
|
j)
|
Prior to May 1, 2012: Miscellaneous
Metal Parts
and Products Coating
|
|
|
1)
|
Clear coating
|
0.52
|
(4.3)
|
|
|
|
0.52*
|
(4.3)*
|
|
|
2)
|
Extreme performance coating
|
|
|
|
A)
|
Air dried
|
0.42
|
(3.5)
|
|
|
|
|
0.42*
|
(3.5)*
|
|
|
|
|
|
|
|
|
B)
|
Baked
|
0.42
|
(3.5)
|
|
|
|
|
0.40*
|
(3.3)*
|
|
|
3)
|
Steel pail and drum interior
coating
|
0.52
|
(4.3)
|
|
|
|
0.52*
|
(4.3)*
|
|
|
4)
|
All other coatings
|
|
|
|
A)
|
Air dried
|
0.42
|
(3.5)
|
|
|
|
|
0.40*
|
(3.3)*
|
|
|
|
B)
|
Baked
|
0.36
|
(3.0)
|
|
|
|
|
0.34*
|
(2.8)*
|
|
|
5)
|
Marine engine coating
|
|
|
|
A)
|
Air dried
|
0.42
|
(3.5)
|
|
|
|
|
0.42*
|
(3.5)*
|
|
|
B)
|
Baked
|
|
|
|
|
|
|
i)
|
Primer/Topcoat
|
0.42
|
(3.5)
|
|
|
|
|
|
0.42*
|
(3.5)*
|
|
|
|
|
ii)
|
Corrosion resistant basecoat
|
0.42
|
(3.5)
|
|
|
|
|
|
0.28*
|
(2.3)*
|
|
|
|
C)
|
Clear Coating
|
0.52
|
(4.3)
|
|
|
|
|
0.52*
|
(4.3)*
|
|
|
6)
|
Metallic Coating
|
|
|
|
A)
|
Air dried
|
0.42
|
(3.5)
|
|
|
|
|
0.42*
|
(3.5)*
|
|
|
|
B)
|
Baked
|
0.36
|
(3.0)
|
|
|
|
|
0.36
|
(3.0)*
|
|
|
|
|
|
|
|
|
|
|
7) Definitions
A) For purposes of subsection (j)(5) of this Section, the
following terms are defined:
i) "Corrosion resistant basecoat" means, for purposes
of subsection (j)(5)(B)(ii) of this Section, a water-borne epoxy coating
applied via an electrodeposition process to a metal surface prior to spray
coating, for the purpose of enhancing corrosion resistance.
ii) "Electrodeposition process" means, for purposes of
subsection (j)(5) of this Section, a water-borne dip coating process in which
opposite electrical charges are applied to the substrate and the coating. The
coating is attracted to the substrate due to the electrochemical potential
difference that is created.
iii) "Marine engine coating" means, for purposes of
subsection (j)(5) of this Section, any extreme performance protective,
decorative or functional coating applied to an engine that is used to propel
watercraft.
B) For purposes of subsection (j)(6) of this Section,
"metallic coating" means a coating which contains more than ¼ lb/gal
of metal particles, as applied.
BOARD NOTE:
On and after May 1, 2012, the limitations in Section 218.204(q) shall apply to
this category of coating.
k)
|
Heavy Off-Highway Vehicle
Products Coating
|
kg/l
|
lb/gal
|
|
|
1)
|
Extreme performance prime coat
|
0.42
|
(3.5)
|
|
|
|
0.42*
|
(3.5)*
|
|
|
2)
|
Extreme performance topcoat
(air dried)
|
0.42
|
(3.5)
|
|
|
|
0.42*
|
(3.5)*
|
|
|
3)
|
Final repair coat (air dried)
|
0.42
|
(3.5)
|
|
|
|
0.42*
|
(3.5)*
|
4) All
other coatings are subject to the emission limitations for miscellaneous metal
parts and products coatings in subsection (j).
l)
|
Wood Furniture Coating
|
|
|
|
|
1)
|
Limitations before March 15,
1998:
|
kg/l
|
lb/gal
|
|
|
|
|
|
|
|
|
A)
|
Clear topcoat
|
0.67
|
(5.6)
|
|
|
|
B)
|
Opaque stain
|
0.56
|
(4.7)
|
|
|
|
C)
|
Pigmented coat
|
0.60
|
(5.0)
|
|
|
|
D)
|
Repair coat
|
0.67
|
(5.6)
|
|
|
|
E)
|
Sealer
|
0.67
|
(5.6)
|
|
|
|
F)
|
Semi-transparent stain
|
0.79
|
(6.6)
|
|
|
|
G)
|
Wash coat
|
0.73
|
(6.1)
|
BOARD NOTE: Prior to March 15,
1998, an owner or operator of a wood furniture coating operation subject to
this Section shall apply all coatings, with the exception of no more than 37.8
l (10 gal) of coating per day used for touch-up and repair operations, using one
or more of the following application systems: airless spray application
system, air-assisted airless spray application system, electrostatic spray
application system, electrostatic bell or disc spray application system, heated
airless spray application system, roller coating, brush or wipe coating
application system, dip coating application system or high volume low pressure
(HVLP) application system.
2) On and after March 15, 1998, wood furniture sealers and
topcoats must comply with one of the limitations specified in subsections
(l)(2)(A) through (E):
|
|
|
kg VOM/
kg solids
|
lb VOM/
lb solids
|
|
|
|
A)
|
Topcoat
|
0.8
|
(0.8)
|
|
|
|
B)
|
Sealers and topcoats with the
following limits:
|
|
|
|
|
|
|
i)
|
Sealer other than acid-cured
alkyd amino vinyl sealer
|
1.9
|
(1.9)
|
|
|
|
|
ii)
|
Topcoat other than acid-cured
alkyd amino conversion varnish topcoat
|
1.8
|
(1.8)
|
|
|
|
|
iii)
|
Acid-cured alkyd amino vinyl
sealer
|
2.3
|
(2.3)
|
|
|
|
|
iv)
|
Acid-cured alkyd amino
conversion varnish topcoat
|
2.0
|
(2.0)
|
C) Meet the provisions of Section 218.215 of this Subpart for use
of an averaging approach;
D) Achieve a reduction in emissions equivalent to the requirements
of subsection (l)(2)(A) or (B) of this Section, as calculated using Section
218.216 of this Subpart; or
E) Use a combination of the methods specified in subsections
(l)(2)(A) through (D) of this Section.
3) Other wood furniture coating limitations on and after March
15, 1998:
|
|
|
kg/l
|
lb/gal
|
|
|
A)
|
Opaque stain
|
0.56
|
(4.7)
|
|
|
|
B)
|
Non-topcoat pigmented coat
|
0.60
|
(5.0)
|
|
|
|
C)
|
Repair coat
|
0.67
|
(5.6)
|
|
|
|
D)
|
Semi-transparent stain
|
0.79
|
(6.6)
|
|
|
|
E)
|
Wash coat
|
0.73
|
(6.1)
|
4) Other wood furniture coating requirements on and after March
15, 1998:
A) No source subject to the limitations of subsection (l)(2) or
(3) of this Section and utilizing one or more wood furniture coating spray
booths shall use strippable spray booth coatings containing more than 0.8 kg
VOM/kg solids (0.8 lb VOM/lb solids), as applied.
B) Any source subject to the limitations of subsection (l)(2) or
(3) of this Section shall comply with the requirements of Section 218.217 of
this Subpart.
C) Any source subject to the limitations of subsection (l)(2)(A)
or (B) of this Section and utilizing one or more continuous coaters shall, for
each continuous coater, use an initial coating which complies with the
limitations of subsection (l)(2)(A) or (B) of this Section. The viscosity of
the coating in each reservoir shall always be greater than or equal to the
viscosity of the initial coating in the reservoir. The owner or operator
shall:
i) Monitor the viscosity of the coating in the reservoir with a
viscosity meter or by testing the viscosity of the initial coating and
retesting the coating in the reservoir each time solvent is added;
ii) Collect and record the reservoir viscosity and the amount and
weight of VOM per weight of solids of coating and solvent each time coating or
solvent is added; and
iii) Maintain these records at the source for a period of three
years.
m)
|
Existing Diesel-Electric
Locomotive Coating Lines in Cook County
|
kg/l
|
lb/gal
|
|
|
1)
|
Extreme performance prime coat
|
0.42
|
(3.5)
|
|
|
|
0.42*
|
(3.5)*
|
|
|
2)
|
Extreme performance top-coat
(air dried)
|
0.42
|
(3.5)
|
|
|
|
0.42*
|
(3.5)*
|
|
|
3)
|
Final repair coat (air dried)
|
0.42
|
(3.5)
|
|
|
|
0.42*
|
(3.5)*
|
|
|
4)
|
High-temperature aluminum
coating
|
0.72
|
(6.0)
|
|
|
|
0.72*
|
(6.0)*
|
|
|
5)
|
All other coatings
|
0.36
|
(3.0)
|
|
|
|
0.36*
|
(3.0)*
|
n)
|
Prior to May 1, 2012: Plastic
Parts Coating: Automotive/Transportation
|
kg/l
|
lb/gal
|
|
|
1)
|
Interiors
|
|
|
|
|
|
A)
|
Baked
|
|
|
|
|
|
|
i)
|
Color coat
|
0.49*
|
(4.1)*
|
|
|
|
|
ii)
|
Primer
|
0.46*
|
(3.8)*
|
|
|
|
B)
|
Air dried
|
|
|
|
|
|
|
i)
|
Color coat
|
0.38*
|
(3.2)*
|
|
|
|
|
ii)
|
Primer
|
0.42*
|
(3.5)*
|
|
|
2)
|
Exteriors (flexible and
non-flexible)
|
|
|
|
|
|
A)
|
Baked
|
|
|
|
|
|
|
i)
|
Primer
|
0.60*
|
(5.0)*
|
|
|
|
|
ii)
|
Primer non-flexible
|
0.54*
|
(4.5)*
|
|
|
|
|
iii)
|
Clear coat
|
0.52*
|
(4.3)*
|
|
|
|
|
iv)
|
Color coat
|
0.55*
|
(4.6)*
|
|
|
|
B)
|
Air dried
|
|
|
|
|
|
|
i)
|
Primer
|
0.66*
|
(5.5)*
|
|
|
|
|
ii)
|
Clear coat
|
0.54*
|
(4.5)*
|
|
|
|
|
iii)
|
Color coat (red & black)
|
0.67*
|
(5.6)*
|
|
|
|
|
iv)
|
Color coat (others)
|
0.61*
|
(5.1)*
|
|
|
3)
|
Specialty
|
|
|
|
|
|
A)
|
Vacuum metallizing basecoats,
texture base coats
|
0.66*
|
(5.5)*
|
|
|
|
B)
|
Black coatings, reflective
argent coatings, air bag cover coatings, and soft coatings
|
0.71*
|
(5.9)*
|
|
|
|
C)
|
Gloss reducers, vacuum
metallizing topcoats, and texture topcoats
|
0.77*
|
(6.4)*
|
|
|
|
D)
|
Stencil coatings, adhesion primers,
ink pad coatings, electrostatic prep coatings, and resist coatings
|
0.82*
|
(6.8)*
|
|
|
|
E)
|
Headlamp lens coatings
|
0.89*
|
(7.4)*
|
BOARD NOTE: On and after May 1,
2012, the limitations in Section 218.240(q) shall apply to this category of coating.
o)
|
Prior to May 1, 2012: Plastic
Parts Coating: Business Machine
|
kg/l
|
lb/gal
|
|
|
1)
|
Primer
|
0.14*
|
(1.2)*
|
|
|
2)
|
Color coat (non-texture coat)
|
0.28*
|
(2.3)*
|
|
|
3)
|
Color coat (texture coat)
|
0.28*
|
(2.3)*
|
|
|
4)
|
Electromagnetic interference/radio
frequency interference (EMI/RFI) shielding coatings
|
0.48*
|
(4.0)*
|
|
|
5)
|
Specialty coatings
|
|
|
|
|
|
A)
|
Soft coat
|
0.52*
|
(4.3)*
|
|
|
|
B)
|
Plating resist
|
0.71*
|
(5.9)*
|
|
|
|
C)
|
Plating sensitizer
|
0.85*
|
(7.1)*
|
BOARD NOTE:
On and after May 1, 2012, the limitations in Section 218.204(q) shall apply to
this category of coating.
p) Flat Wood Paneling Coatings. On and after August 1, 2010,
flat wood paneling coatings shall comply with one of the following limitations:
1) 0.25 kg VOM/1 of coatings (2.1 lb VOM/gal coatings); or
2)
0.35 kg VOM/1 solids (2.9 lb VOM/gal solids).
q) Miscellaneous Metal Parts and Products Coatings and Plastic
Parts and Products Coatings On and After May 1, 2012. On and after May 1, 2012,
the owner or operator of a miscellaneous metal or plastic parts coating line
shall comply with the limitations in this subsection (q). The limitations in
this subsection (q) shall not apply to aerosol coating products, powder
coatings, or primer sealants and ejection cartridge sealants used in ammunition
manufacturing. Primer sealants and ejection cartridge sealants shall instead
be regulated under Subpart TT of this Part.
1) Metal Parts and Products. For purposes of this subsection
(q)(1), "corrosion resistant basecoat" means a water-borne epoxy
coating applied via an electrodeposition process to a metal surface prior to
spray coating, for the purpose of enhancing corrosion resistance. The
limitations in this subsection (q)(1) shall not apply to stencil coats,
safety-indicating coatings, solid-film lubricants, electric-insulating and
thermal-conducting coatings, magnetic data storage disk coatings, and plastic
extruded onto metal parts to form a coating. The limitations in Section
218.219, however, shall apply to these coatings unless specifically excluded in
Section 218.219.
|
kg/l
(lb/gal)
coatings
|
kg/l
(lb/gal)
solids
|
|
|
A)
|
General one component coating
|
|
|
|
|
|
|
|
|
|
|
|
i)
|
Air dried
|
0.34
|
0.54
|
|
|
|
|
|
(2.8)
|
(4.52)
|
|
|
|
|
|
|
|
|
|
|
ii)
|
Baked
|
0.28
|
0.40
|
|
|
|
|
|
(2.3)
|
(3.35)
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
B)
|
General multi-component
coating
|
|
|
|
|
|
|
|
|
|
|
|
i)
|
Air dried
|
0.34
|
0.54
|
|
|
|
|
|
(2.8)
|
(4.52)
|
|
|
|
|
|
|
|
|
|
|
ii)
|
Baked
|
0.28
|
0.40
|
|
|
|
|
|
(2.3)
|
(3.35)
|
|
|
|
|
|
|
|
|
|
C)
|
Camouflage coating
|
0.42
|
0.80
|
|
|
|
|
|
(3.5)
|
(6.67)
|
|
|
|
|
|
|
|
|
|
D)
|
Electric-insulating varnish
|
0.42
|
0.80
|
|
|
|
|
|
(3.5)
|
(6.67)
|
|
|
|
|
|
|
|
|
|
E)
|
Etching filler
|
0.42
|
0.80
|
|
|
|
|
|
(3.5)
|
(6.67)
|
|
|
|
|
|
|
|
|
|
F)
|
Extreme high-gloss coating
|
|
|
|
|
|
|
|
|
|
|
|
|
i)
|
Air dried
|
0.42
|
0.80
|
|
|
|
|
|
(3.5)
|
(6.67)
|
|
|
|
|
|
|
|
|
|
|
ii)
|
Baked
|
0.36
|
0.61
|
|
|
|
|
|
(3.0)
|
(5.06)
|
|
|
|
|
|
|
|
|
|
G)
|
Extreme performance coating
|
|
|
|
|
|
|
|
|
|
|
|
|
i)
|
Air dried
|
0.42
|
0.80
|
|
|
|
|
|
(3.5)
|
(6.67)
|
|
|
|
|
|
|
|
|
|
|
ii)
|
Baked
|
0.36
|
0.61
|
|
|
|
|
|
(3.0)
|
(5.06)
|
|
|
|
|
|
|
|
|
|
H)
|
Heat-resistant coating
|
|
|
|
|
|
|
|
|
|
|
|
i)
|
Air dried
|
0.42
|
0.80
|
|
|
|
|
(3.5)
|
(6.67)
|
|
|
|
|
|
|
|
|
|
ii)
|
Baked
|
0.36
|
0.61
|
|
|
|
|
(3.0)
|
(5.06)
|
|
|
|
|
|
|
|
|
I)
|
High performance architectural
coating
|
0.42
(3.5)
|
0.80
(6.67)
|
|
|
|
|
|
|
|
|
J)
|
High temperature coating
|
0.42
|
0.80
|
|
|
|
|
(3.5)
|
(6.67)
|
|
|
|
|
|
|
|
|
K)
|
Metallic coating
|
|
|
|
|
|
|
|
|
|
|
|
i)
|
Air dried
|
0.42
|
0.80
|
|
|
|
|
(3.5)
|
(6.67)
|
|
|
|
|
|
|
|
|
|
ii)
|
Baked
|
0.36
|
0.61
|
|
|
|
|
(3.0)
|
(5.06)
|
|
|
|
|
|
|
|
|
L)
|
Military specification coating
|
|
|
|
|
|
|
|
|
|
|
|
i)
|
Air dried
|
0.34
|
0.54
|
|
|
|
|
(2.8)
|
(4.52)
|
|
|
|
|
|
|
|
|
|
ii)
|
Baked
|
0.28
|
0.40
|
|
|
|
|
(2.3)
|
(3.35)
|
|
|
|
|
|
|
|
|
M)
|
Mold-seal coating
|
0.42
|
0.80
|
|
|
|
|
(3.5)
|
(6.67)
|
|
|
|
|
|
|
|
|
N)
|
Pan backing coating
|
0.42
|
0.80
|
|
|
|
|
(3.5)
|
(6.67)
|
|
|
|
|
|
|
|
|
O)
|
Prefabricated architectural
coating: multi-component
|
|
|
|
|
|
|
|
|
|
|
|
i)
|
Air dried
|
0.42
|
0.80
|
|
|
|
|
(3.5)
|
(6.67)
|
|
|
|
|
|
|
|
|
|
ii)
|
Baked
|
0.28
|
0.40
|
|
|
|
|
(2.3)
|
(3.35)
|
|
|
|
|
|
|
|
|
P)
|
Prefabricated architectural
|
|
|
|
|
|
coating: one-component
|
|
|
|
|
|
|
|
|
|
|
|
i)
|
Air dried
|
0.42
|
0.80
|
|
|
|
|
(3.5)
|
(6.67)
|
|
|
|
|
|
|
|
|
|
ii)
|
Baked
|
0.28
|
0.40
|
|
|
|
|
(2.3)
|
(3.35)
|
|
|
|
|
|
|
|
|
Q)
|
Pretreatment coating
|
0.42
|
0.80
|
|
|
|
|
(3.5)
|
(6.67)
|
|
|
|
|
|
|
|
|
R)
|
Repair coats and touch-up
coatings
|
|
|
|
|
|
|
|
|
|
|
|
i)
|
Air dried
|
0.42
|
|
|
|
|
|
(3.5)
|
|
|
|
|
|
|
|
|
|
|
ii)
|
Baked
|
0.36
|
|
|
|
|
|
(3.01)
|
|
|
|
|
|
|
|
|
|
S)
|
Silicone release coating
|
0.42
|
0.80
|
|
|
|
|
(3.5)
|
(6.67)
|
|
|
|
|
|
|
|
|
T)
|
Solar-absorbent coating
|
|
|
|
|
|
|
|
|
|
|
|
i)
|
Air dried
|
0.42
|
0.80
|
|
|
|
|
(3.5)
|
(6.67)
|
|
|
|
|
|
|
|
|
|
ii)
|
Baked
|
0.36
|
0.61
|
|
|
|
|
(3.0)
|
(5.06)
|
|
|
|
|
|
|
|
|
U)
|
Vacuum-metalizing coating
|
0.42
|
0.80
|
|
|
|
|
(3.5)
|
(6.67)
|
|
|
|
|
|
|
|
|
V)
|
Drum coating, new, exterior
|
0.34
|
0.54
|
|
|
|
|
(2.8)
|
(4.52)
|
|
|
|
|
|
|
|
|
W)
|
Drum coating, new, interior
|
0.42
|
0.80
|
|
|
|
|
(3.5)
|
(6.67)
|
|
|
|
|
|
|
|
|
X)
|
Drum coating, reconditioned,
exterior
|
0.42
(3.5)
|
0.80
(6.67)
|
|
|
|
|
|
|
|
|
Y)
|
Drum coating, reconditioned,
interior
|
0.50
(4.2)
|
1.17
(9.78)
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Z)
|
Ammunition Sealants
|
|
|
|
|
|
|
|
|
|
|
|
i)
|
Air dried
|
0.42
|
0.80
|
|
|
|
|
(3.5)
|
(6.67)
|
|
|
|
|
|
|
|
|
|
ii)
|
Baked
|
0.36
|
0.61
|
|
|
|
|
(3.0)
|
(5.06)
|
|
|
|
|
|
|
|
|
AA)
|
Electrical switchgear compartment
coatings
|
|
|
|
|
|
|
|
|
|
|
|
i)
|
Air dried
|
0.42
|
0.80
|
|
|
|
|
(3.5)
|
(6.67)
|
|
|
|
|
|
|
|
|
|
ii)
|
Baked
|
0.36
|
0.61
|
|
|
|
|
(3.0)
|
(5.06)
|
|
|
BB)
|
All other coatings
|
|
|
|
|
|
|
|
|
|
|
|
i)
|
Air dried
|
0.40
|
0.73
|
|
|
|
|
(3.3)
|
(5.98)
|
|
|
|
|
|
|
|
|
|
ii)
|
Baked
|
0.34
|
0.54
|
|
|
|
|
(2.8)
|
(4.52)
|
|
|
|
|
|
|
|
|
2) Plastic
Parts and Products: Miscellaneous. For purposes of this subsection (q)(2),
miscellaneous plastic parts and products are plastic parts and products that
are not subject to subsection (q)(3), (q)(4), (q)(5), or (q)(6) of this
Section. The limitations in subsection (q)(2) shall not apply to touch-up and
repair coatings; stencil coats applied on clear or transparent substrates;
clear or translucent coatings; coatings applied at a paint manufacturing
facility while conducting performance tests on the coatings; any individual
coating category used in volumes less than 189.2 liters (50 gallons) in any one
calendar year, if the total usage of all such coatings does not exceed 756.9
liters (200 gallons) per calendar year per source and substitute compliant
coatings are not available; reflective coatings applied to highway cones; mask
coatings that are less than 0.5 mm thick (dried) if the area coated is less
than 25 square inches; electromagnetic interference/radio frequency
interference (EMI/RFI) shielding coatings; and heparin-benzalkonium chloride
(HBAC)-containing coatings applied to medical devices if the total usage of all
such coatings does not exceed 378.4 liters (100 gallons) per calendar year per
source. The limitations in Section 218.219, however, shall apply to such
coatings unless specifically excluded in Section 218.219.
|
|
|
kg/l (lb/gal) coatings
|
kg/l
(lb/gal)
solids
|
|
|
|
|
|
|
|
A)
|
General one component coating
|
0.28
|
0.40
|
|
|
|
(2.3)
|
(3.35)
|
|
|
|
|
|
|
|
|
|
B)
|
General multi-component
|
0.42
|
0.80
|
|
|
|
|
|
(3.5)
|
(6.67)
|
|
|
|
|
|
|
|
|
C)
|
Electric dissipating coatings
|
0.80
|
8.96
|
|
|
|
and shock-free coatings
|
(6.7)
|
(74.7)
|
|
|
|
|
|
|
|
|
D)
|
Extreme performance
(2-pack coatings)
|
0.42
(3.5)
|
0.80
(6.67)
|
|
|
|
|
|
|
|
|
E)
|
Metallic coating
|
0.42
|
0.80
|
|
|
|
|
(3.5)
|
(6.67)
|
|
|
|
|
|
|
|
|
F)
|
Military specification coating
|
|
|
|
|
|
|
|
|
|
|
|
i)
|
1-pack coatings
|
0.28
|
0.54
|
|
|
|
|
(2.3)
|
(4.52)
|
|
|
|
|
|
|
|
|
|
ii)
|
2-pack coatings
|
0.42
|
0.80
|
|
|
|
|
(3.5)
|
(6.67)
|
|
|
|
|
|
|
|
|
G)
|
Mold-seal coating
|
0.76
|
5.24
|
|
|
|
|
(6.3)
|
(43.7)
|
|
|
|
|
|
|
|
|
H)
|
Multi-colored coating
|
0.68
|
3.04
|
|
|
|
|
(5.7)
|
(25.3)
|
|
|
|
|
|
|
|
|
I)
|
Optical coating
|
0.80
|
8.96
|
|
|
|
|
(6.7)
|
(74.7)
|
|
|
|
|
|
|
|
|
J)
|
Vacuum-metalizing coating
|
0.80
|
8.96
|
|
|
|
|
(6.7)
|
(74.7)
|
|
|
|
|
|
|
|
|
|
3) Plastic Parts and Products:
Automotive/Transportation
|
|
|
kg/l (lb/gal) coatings
|
kg/l
(lb/gal)
solids
|
|
|
|
|
|
|
|
|
A)
|
High bake coatings −
interior and exterior parts
|
|
|
|
|
|
|
|
|
|
|
|
i)
|
Flexible primer
|
0.54
|
1.39
|
|
|
|
|
(4.5)
|
(11.58)
|
|
|
|
|
|
|
|
|
|
ii)
|
Non-flexible primer
|
0.42
|
0.80
|
|
|
|
|
(3.5)
|
(6.67)
|
|
|
|
|
|
|
|
|
|
iii)
|
Basecoats
|
0.52
|
1.24
|
|
|
|
|
(4.3)
|
(10.34)
|
|
|
|
|
|
|
|
|
|
|
iv)
|
Clear coat
|
0.48
|
1.05
|
|
|
|
|
|
(4.0)
|
(8.76)
|
|
|
|
|
|
|
|
|
|
|
v)
|
Non-basecoat/clear coat
|
0.52
|
1.24
|
|
|
|
|
(4.3)
|
(10.34)
|
|
|
|
|
|
|
|
|
B)
|
Low bake/air dried coatings
− exterior parts
|
|
|
|
|
|
|
|
|
|
|
|
i)
|
Primers
|
0.58
|
1.66
|
|
|
|
|
(4.8)
|
(13.80)
|
|
|
|
|
|
|
|
|
|
ii)
|
Basecoat
|
0.60
|
1.87
|
|
|
|
|
(5.0)
|
(15.59)
|
|
|
|
|
|
|
|
|
|
iii)
|
Clear coats
|
0.54
|
1.39
|
|
|
|
|
(4.5)
|
(11.58)
|
|
|
|
|
|
|
|
|
|
|
iv)
|
Non-basecoat/clear coat
|
0.60
|
1.87
|
|
|
|
|
|
(5.0)
|
(15.59)
|
|
|
|
|
|
|
|
|
|
C)
|
Low bake/air dried coatings
− interior parts
|
|
|
|
|
|
|
|
|
|
|
|
i)
|
Color coat
|
0.38
|
0.67
|
|
|
|
|
(3.2)
|
(5.66)
|
|
|
|
|
|
|
|
|
|
ii)
|
Primer
|
0.42
|
0.80
|
|
|
|
|
(3.5)
|
(6.67)
|
|
|
|
|
|
|
|
|
D)
|
Touchup and repair coatings
|
0.62
|
2.13
|
|
|
|
|
(5.2)
|
(17.72)
|
|
|
|
|
|
|
|
|
|
|
E)
|
Specialty
|
|
|
|
|
|
|
|
|
|
|
|
i)
|
Vacuum metallizing basecoats
|
0.66
(5.5)
|
2.62
(21.8)
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
ii)
|
Vacuum metallizing topcoats
|
0.77
(6.4)
|
6.06
(49.1)
|
|
|
|
|
|
|
|
|
F)
|
Red, yellow, and black
coatings: Subject coating lines shall comply with a limit determined by
multiplying the appropriate limit in subsections (q)(3)(A) through (q)(3)(C)
of this Section by 1.15.
|
4) Plastic
Parts and Products: Business Machine. The limitations of this subsection
(q)(4) shall not apply to vacuum metallizing coatings, gloss reducers, texture
topcoats, adhesion primers, electrostatic preparation coatings, stencil coats,
and resist coats other than plating resist coats. The limitations in Section
218.219, however, shall apply to such coatings unless specifically excluded in
Section 218.219.
|
|
|
kg/l (lb/gal) coatings
|
kg/l
(lb/gal)
solids
|
|
|
|
|
|
|
|
A)
|
Primers
|
0.35
|
0.57
|
|
|
|
(2.9)
|
(4.80)
|
|
|
|
|
|
|
|
|
|
B)
|
Topcoat
|
0.35
|
0.57
|
|
|
|
|
|
(2.9)
|
(4.80)
|
|
|
|
|
|
|
|
|
C)
|
Color coat (texture coat)
|
0.28
|
0.40
|
|
|
|
|
(2.3)
|
(4.80)
|
|
|
|
|
|
|
|
|
D)
|
Color coat (non-texture coat)
|
0.28
|
0.40
|
|
|
|
|
(2.3)
|
(4.80)
|
|
|
|
|
|
|
|
|
E)
|
Texture coats other than color
texture coats
|
0.35
(2.9)
|
0.57
(4.80)
|
|
|
|
|
|
|
|
|
F)
|
EMI/RFI shielding coatings
|
0.48
|
1.05
|
|
|
|
|
(4.0)
|
(8.76)
|
|
|
|
|
|
|
|
|
|
G)
|
Fog coat
|
0.26
|
0.38
|
|
|
|
|
(2.2)
|
(3.14)
|
|
|
|
|
|
|
|
|
|
H)
|
Touchup and repair
|
0.35
|
0.57
|
|
|
|
|
|
|
|
|
|
5) Pleasure
Craft Surface Coatings
|
|
|
|
kg/l (lb/gal) coatings
|
kg/l
(lb/gal)
solids
|
|
|
A)
|
Extreme high gloss coating
− topcoat
|
0.60
|
1.88
|
|
|
|
|
(5.0)
|
(15.6)
|
|
|
|
|
|
|
|
|
|
B)
|
High gloss coating −
topcoat
|
0.42
|
0.80
|
|
|
|
|
|
|
(3.5)
|
(6.7)
|
|
|
|
|
|
|
|
|
|
|
C)
|
Pretreatment wash primer
|
0.78
|
6.67
|
|
|
|
|
|
|
(6.5)
|
(55.6)
|
|
|
|
|
|
|
|
|
|
D)
|
Finish primer/surfacer
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Prior to January 1, 2014
|
0.60
|
1.88
|
|
|
|
|
|
(5.0)
|
(15.6)
|
|
|
|
|
|
|
|
|
|
|
|
On and after January 1, 2014
|
0.42
|
0.80
|
|
|
|
|
|
(3.5)
|
(6.7)
|
|
|
|
|
|
|
|
|
|
E)
|
High build primer/surfacer
|
0.34
|
0.55
|
|
|
|
|
|
(2.8)
|
(4.6)
|
|
|
|
|
|
|
|
|
|
F)
|
Aluminum substrate antifoulant
coating
|
0.56
(4.7)
|
1.53
(12.8)
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
G)
|
Other substrate antifoulant
coating
|
0.40
|
0.73
|
|
|
|
|
|
|
(3.3)
|
(5.8)
|
|
|
|
|
|
|
|
|
|
H)
|
Antifouling Sealer/Tie Coat
|
0.42
|
0.80
|
|
|
|
|
|
(3.5)
|
(6.7)
|
|
|
|
|
|
|
|
|
|
I)
|
All other pleasure craft
surface coatings for metal or plastic
|
0.42
(3.5)
|
0.80
(6.7)
|
|
|
|
|
|
|
|
|
|
|
6) Motor Vehicle Materials
|
|
|
|
kg/l (lb/gal) coatings
|
|
|
|
A)
|
Cavity wax
|
0.65
|
|
|
|
|
|
(5.42)
|
|
|
|
|
|
|
|
|
|
|
B)
|
Sealer
|
0.65
|
|
|
|
|
|
|
|
(5.42)
|
|
|
|
|
|
|
|
|
|
|
|
C)
|
Deadener
|
0.65
|
|
|
|
|
|
|
|
(5.42)
|
|
|
|
|
|
|
|
|
|
|
D)
|
Gasket/gasket sealing material
|
0.20
|
|
|
|
|
|
|
(1.67)
|
|
|
|
|
|
|
|
|
|
|
E)
|
Underbody coating
|
0.65
|
|
|
|
|
|
|
(5.42)
|
|
|
|
|
|
|
|
|
|
|
F)
|
Trunk interior coating
|
0.65
|
|
|
|
|
|
|
(5.42)
|
|
|
|
|
|
|
|
|
|
|
G)
|
Bedliner
|
0.20
|
|
|
|
|
|
|
|
(1.67)
|
|
|
|
|
|
|
|
|
|
|
H)
|
Lubricating wax/compound
|
0.70
(5.84)
|
|
|
|
|
|
|
|
|
|
|
|
(Source: Amended at 35 Ill.
Reg. 13473, effective July 27, 2011)